High resistivity and low core loss of intergranular insulated Fe–6.5wt.%Si/SiO 2 composite compacts

z y wu
DOI: https://doi.org/10.1016/j.matdes.2015.10.087
IF: 9.417
2016-01-01
Materials & Design
Abstract:Intergranular insulated Fe-6.5 wt%Si/SiO2 composite compacts were prepared by in-situ chemical deposition combined with a subsequent spark plasma sintering process. Most of the conductive Fe-6.5 wt.%Si alloy particles were coated with SiO2 insulating layer in Fe-6.5 wt%Si/SiO2 composite compacts. The presence of SiO2 insulating layer increased the resistivity by two orders of magnitude for intergranular insulated Fe-6.5 wt%Si/SiO2 composite compacts (4.8 x 10(-5) Omega.m) compared with that of Fe-6.5 wt.%Si compacts without SiO2 insulating layer (9.7 x 10(-7) Omega.m). In addition, most of the eddy currents could be confined in the SiO2-coated Fe-6.5 wt.%Si particles, which equated to reducing the effective radius of eddy current in Fe-6.5 wt.%Si alloy. So, the intergranular insulated Fe-6.5 waSi/SiO2 composite compacts presented a lower core loss compared with that of Fe-6.5 wt%Si compacts without SiO2 insulating layer or traditional Fe-6.5 wt.%Si electrical steels at medium and high frequencies. Good soft magnetic properties were also obtained for the intergranular insulated Fe-6.5 wt%Si/SiO2 composite compacts, with a saturation magnetization of 164.6 emu/g, a coercive force of 12 Oe, and a relative permeability of 3.2 x 10(3) at 50 Hz. The intergranular insulated Fe-6.5 wt%Si/SiO2 composite compacts provide valuable inspiration for developing new high silicon electrical steel cores with low core loss and excellent magnetic and electric properties. (C) 2015 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?