Core loss reduction in Fe–6.5wt.%Si/SiO 2 core–shell composites by ball milling coating and spark plasma sintering

zhaoyang wu,xi an fan,jian wang,guangqiang li,zhanghua gan,zhan zhang
DOI: https://doi.org/10.1016/j.jallcom.2014.07.217
IF: 6.2
2014-01-01
Journal of Alloys and Compounds
Abstract:•The Fe–6.5wt.%Si/SiO2 core–shell composite powders and compacts have been prepared.•The microstructure, magnetic and electrical properties of the compacts were investigated.•The Fe–6.5wt.%Si/SiO2 compacts have a high ρ (1.5×10−5Ωm) and low core loss (3.7W/kg (P2/400)).•The core–shell structures show a prospect to increase ρ and reduce core loss of Fe–6.5wt.%Si alloys.