The segregation behaviors of fine coal particles in a coal beneficiation fluidized bed

qinggong wang,weidi yin,bin zhao,hairui yang,junfu lu,lubin wei
DOI: https://doi.org/10.1016/j.fuproc.2014.02.015
IF: 8.129
2014-01-01
Fuel Processing Technology
Abstract:The segregation behaviors of fine coal particles in a coal beneficiation fluidized bed (CBFB) were investigated in this work. The size range of 1–8mm was taken into account and three separate size fractions were studied comparatively in the experiments, e.g. 1–2mm, 3–5.5mm and 5.5–8mm. Both a clean coal sample and a gangue sample were used as the processed material to study the segregation behaviors of both light particles and heavy particles. The dense bed was divided as seven layers from bottom to top and the particle distribution in each layer for each sample was fully demonstrated. The influences of the particle density, particle size and the fluidized air velocity were revealed, the segregation patterns under different conditions were compared and the segregation mechanism was carefully analyzed. The results showed that the flotation and sedimentation of the particles in CBFB were still largely influenced by the particle density for the fine size range particles, and density stratification occurred even within each size fraction sample. The weight fraction in each layer showed a quadratic increase along the bed height for the coal particles. For gangue particles, a large fraction deposited in the bottom while the mass proportions in the middle layers also showed an increased tendency. With a decrease of the particle size, both the particle segregation and the density stratification phenomena deteriorated seriously. It was proved that particle feed size should be above 3mm as the separation effect was quite inefficient for finer particles. By increasing the fluidized air velocity, the bed density slightly decreased but the bed turbulence was largely strengthened by the increasing bubble boiling effect. The flotation and sedimentation of the particles in 5.5–8mm were obviously affected while no clear influence occurred to the rest of the two size fractions. Moreover, the results in this work provide a group of data that are quite suitable for CBFB numerical modeling studies.
What problem does this paper attempt to address?