Oxidation Kinetics of the AlPO4 Ceramic Coatings by Pulse Arc Discharge Deposition on SiC–C/C Composites

Jianfeng Huang,Wei Hao,Hejun Li,Qiangang Fu,Liyun Cao,Yongliang Zhang,Cuiyan Li,Lixiong Yin,Haibo Ouyang
DOI: https://doi.org/10.1016/j.vacuum.2014.11.010
IF: 4
2015-01-01
Vacuum
Abstract:An AlPO4 oxidation-protective coating was successfully prepared on SiC pre-coated carbon/carbon composites (SiC-C/C) by pulse arc discharge deposition. The structure and oxidation resistance of the as-prepared AlPO4/SiC multilayer coatings were investigated. The results were confirmed by oxidation experiments performed at 1573 K, 1673 K and 1773 K, which demonstrated that the AlPO4/SiC coating could efficiently protect C/C composites from oxidation at 1773 K for 160 h with a weight loss of only 0.7%. The oxidation activation energy of the coated C/C composites at 1573-1773 K was calculated to be 119.2 kJ mol(-1). (C) 2014 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?