Effects of Different Filler Metals on the Mechanical Behaviors of Gta Welded Aa7a52(T6)

Fengyuan Shu,Yaohui Lv,Yuxin Liu,Jianjun Lin,Zhe Sun,Binshi Xu,Peng He
DOI: https://doi.org/10.1007/s11665-014-1015-7
IF: 2.3
2014-01-01
Journal of Materials Engineering and Performance
Abstract:ER4043, ER5356, and AA7A52 on behalf of the Al-Si, Al-Mg, and Al-Zn-Mg-based welding material, respectively, were chosen as the filler metal to weld AA7A52(T6) plates by GTAW. The variance in mechanical performances of the joints caused by the various filler materials was investigated with reference to the SEM and EDS test results for the weld seam and the fracture surface. Failure was found in the seam for all the welded joints. With regard to the joint obtained with ER4043 welding wire, the total elongation was limited by the brittle intergranular compound Mg2Si of which Mg was introduced by convection mass transfer. As for the other two welds, the content ratio of Zn and Mg was found to play the dominant role in deciding the mechanical properties of the intergranular Mg-Zn compounds which were responsible for the tensile behavior of the joints. The content ratio (wt.%) of beyond 2:1 gave birth to the strengthening phase MgZn2 leading to a ductile fracture. Cr in the seam obtained with AA7A52 filler metal was found to enhance the strength of the joint through isolated particles.
What problem does this paper attempt to address?