Strain Controlled Orbital State And Magnetization In Insulating Lamno3+Delta Films

s l cheng
DOI: https://doi.org/10.1063/1.4919226
IF: 2.877
2015-01-01
Journal of Applied Physics
Abstract:LaMnO3+delta films with various thicknesses were grown on LaAlO3 (001) single crystal substrate to investigate the effect of in-plane compressive strain (similar to-0.57%) on magnetic properties. All films exhibit a blocking temperature T-b at which the zero field cooled magnetization reaches a maximum, indicating the ferromagnetic (FM) nanoclusters are embedded in the background of antiferromagnetic (AFM) matrix. The onset temperature of FM transition T-c and T-b is increased by 24% and 89%, respectively, with the thickness decreasing from 82.4 nm to 9.2 nm. Simultaneously, the saturation magnetization greatly increases by 309%, which is ascribed to the strain-induced transition of AFM to FM phase due to the orbital order structure switching from x(2) - 1/y(2) - 1 [A-type] to (x(2) - y(2)) + (z(2) - 1) [F-type]. (C) 2015 AIP Publishing LLC.
What problem does this paper attempt to address?