Microstructure, Mechanical Properties, and Electrical Resistivities of Mica Glass-Ceramics with Flake Phlogopite and Waste Glass

Yufei Chen,Yan'gai Liu,Xiaowen Wu,Zhaohui Huang,Minghao Fang
DOI: https://doi.org/10.4028/www.scientific.net/kem.602-603.640
2014-01-01
Key Engineering Materials
Abstract:Mica glass-ceramics can be applied in all kinds of electrical equipment, locomotive internal circuits in high-speed rail, ordinary electric locomotive and subway locomotive. In this study, mica glass-ceramics were prepared by sintering process using flake mica and waste glass as the main raw material with low cost. Different mica glass-ceramic samples were fabricated by changing the formula of raw materials, molding process and sintering temperature. X-ray diffraction, scanning electron microscopy, three-point bending test, and balanced-bridge technique were applied to investigate the phase, microstructure, mechanical and electrical resistivities of the samples, respectively. The results show that the optimum sintering temperature is 900 to 1000 °C holding for two hours, the desirable ratio is 70 wt% of mica powder while 30 wt% of glass powder. In that condition the sample could be less porosity, high flexural strength (63.3 MPa) and eligible electrical resistivity (0.4×1013 Ω·cm).
What problem does this paper attempt to address?