Low temperature firing and microwave dielectric properties of BaCaV2O7 ceramics

xuewen jiang,chunchun li,congxue su,zhenhai wei,liang fang
DOI: https://doi.org/10.1016/j.ceramint.2014.12.001
IF: 5.532
2015-01-01
Ceramics International
Abstract:A low-firing microwave dielectric ceramic BaCaV2O7 with orthorhombic structure was fabricated by the conventional solid-state reaction method. The phase purity, microstructure, and microwave dielectric properties were investigated. The optimum densification temperature for the BaCaV2O7 ceramic was 830 degrees C. It showed excellent microwave dielectric properties with a relatively low permittivity (epsilon(r)similar to 8.9), a high quality factor Q(u) x f value of 31,362 GHz and a negative temperature coefficient of resonant frequency (tau(f)) of -68.2 ppm/degrees C. CaTiO3 was added into BaCaV2O7 ceramic to obtain a near zero tau(f). BaCaV2O7 ceramic doped with 5 wt% CaTiO3 sintered at 880 degrees C for 2 h exhibited a near zero tau(f)similar to -3.5 ppm/degrees C with epsilon(r)similar to 9.6, Q(u) x f similar to 26,338 GHz. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
What problem does this paper attempt to address?