In Situ Study of the Initiation of Hydrogen Bubbles at the Aluminium Metal/oxide Interface.

De-Gang Xie,Zhang-Jie Wang,Jun Sun,Ju Li,Evan Ma,Zhi-Wei Shan
DOI: https://doi.org/10.1038/nmat4336
IF: 41.2
2015-01-01
Nature Materials
Abstract:Gas-filled bubbles at the interface between a metal substrate and an oxide coating can cause blistering and eventual cracking of the oxide layer. The microscale mechanisms of how hydrogen bubbles form and grow have now been elucidated.
What problem does this paper attempt to address?