Piezoelectric and Ferroelectric Properties of (1-x)Pb(Sc0.5Ta0.5)O3-xPb(Zr0.52Ti0.48)O3 Relaxor Ferroelectric Ceramics

wei shi,qiang chen,dejun lan,lin chen,wei huang,dingquan xiao,jianguo zhu
DOI: https://doi.org/10.1109/ISAF.2006.4387862
2006-01-01
Abstract:(1-x)Pb(Sc0.5Ta0.5)O3-xPb(Zr0.52Ti0.48)O3 (PSTZT-100x) ceramics were prepared by using conventional oxide processing, and their piezoelectric and ferroelectric properties studied. The results of X-ray diffraction (XRD) suggest that PSTZT-100x ceramics formed a single-phase perovskite structure when 0.1lesxles0.8. The ceramics exhibit relatively good piezoelectric and ferroelectric properties: piezoelectric constant, d33=117 pC/N; planar electromechanical coupling factor, kp=45%, remnant polarization, Pr=14 muC/cm2, coercive field, Ec=0.65 kV/mm. The morphotropic phase boundary (MPB) of PSTZT-100x maybe located at x=0.75 because of the maximum piezoelectric constant d33 achieved at x=0.75. The pinched hysteresis loops were founded for PSTZT-100x ceramics when x>0.7, and it was suggested that the pinched ferroelectric loops due to the pinning effect of the dipolar defects formed in PSTZT-100x ceramics.
What problem does this paper attempt to address?