Abstract:The impact of homogenization time and temperature on microstructures and properties of the as-cast and homogenized Mg-9.0Y-3.0MM-0.6Zr alloy were investigated by optical microscopy, scanning electron microscopy and tensile test. The homogenization parameters were determined. The results indicated that the Mg-9.0Y-3.0MM-0.6Zr as-cast microstructures consisted of phases of α-Mg, Mg12(MM) and Mg24Y5 with an average grain size of 45 μm. 505 and 520°C were too low to make Mg-Y phase dissolve completely. After homogenizing at 535 °C for 18 h, there were only Mg12(MM) phases remained and the grains did not grow up as prolonging the homogenization time, indicating that Mg12(MM) phase could efficaciously restrain grain coarsening. The mechanical properties were not significantly changed after homogenization at 535°C for 18 h, compared with the as-cast alloy. The mechanical properties of the homogenization alloy after extrusion were improved obviously, with σ0.2, σb, δ being 245, 305 MPa and 12.5% respectively. The fracture morphology of the as-cast alloy was similar to the homogenized alloy at room temperature. There were a few dimples on local part of the fracture surface, indicating that brittle fracture was the main fracture mechanism. However, the fracture morphology of extruded alloy presented typical ductile fracture characteristics.
What problem does this paper attempt to address?