The effect of DMDA on the pore-size expansion of mesoporous V-MCM-41 molecular sieves

Junqiang Xu,Wei Chu
DOI: https://doi.org/10.3969/j.issn.1001-8719.2011.02.019
2011-01-01
Abstract:Modified mesoporous V-MCM-41 materials were synthesized by hydrothermal method with cetyltrimethylammonium bromide (CATB) as template and dimethyldecylamine (DMDA) as expanding agent, which were characterized by using BET, XRD, SEM, TEM methods. The pore size expansion effects of V-MCM-41 by direct hydrothermal method and post-hydrothermal treatment were investigated. It was shown that the pore size of V-MCM-41 could be changed with the different amount of DMDA in its synthesis, the range of pore size was 3.94-5.49 nm. The pore size didn't increase with the increase of DMDA amounts. The use of DMDA in post-hydrothermal treatment made the pore size of V-MCM-41 from 3.94 nm prepared under conventional hydrothermal synthesis up to 6.62 nm, 68% improvement and with relatively narrow pore-size distributions successfully. The SEM pictures of V-MCM-41 prepared by post-hydrothermal treatment clearly revealed that the resulting particles were almost perfectly spherical in shape.
What problem does this paper attempt to address?