Cation exchange hybrid membranes from SPPO and multi-alkoxy silicon copolymer: Preparation, properties and diffusion dialysis performances for sodium hydroxide recovery

Xinle Xiao,Cuiming Wu,Peng Cui,Jingyi Luo,Yonghui Wu,Tongwen Xu
DOI: https://doi.org/10.1016/j.memsci.2011.05.057
IF: 9.5
2011-01-01
Journal of Membrane Science
Abstract:Cation exchange hybrid membranes for diffusion dialysis (DD) purpose have been prepared from sol–gel process of multi-alkoxy silicon copolymer (poly(vinyl benzyl chloride-γ-methacryloxypropyl trimethoxy silane)—poly(VBC-co-γ-MPS)) in presence of sulfonated poly(2,6-dimethyl-1,4-phenylene oxide) (SPPO). The hybrid membranes possess high thermal stability, mechanical strength, strong alkali and swelling resistance. Thermal initial decomposition temperatures are in the range of 233–245°C. Tensile strength (TS) ranges from 23MPa to 41MPa and elongation at break (Eb) is in the range of 11–50%. The swelling behavior of the membranes is better suppressed as poly(VBC-co-γ-MPS) content increases. The hybrid membranes have been successfully applied for DD recovery of sodium hydroxide (NaOH) from the mixture of NaOH and sodium tungstate (Na2WO4). The separation factor (S) of hybrid membranes can reach as high as 301.5 at 25°C. The pure SPPO membrane, as a comparison membrane, exhibits much lower S value of 36.2.
What problem does this paper attempt to address?