Heat treatment and application of W-Al-containing bainitic steel used for crossing

Chun-lei ZHENG,Bo LU,Fu-cheng ZHANG,Ming ZHANG,Yang-zeng ZHENG
2009-01-01
Abstract:Through replacement of Mo by W and partial replacement of Si by Al in a commercial bainitic steel used for crossing, a new W-Al-containing bainitic steel crossing was developed. The heat treatment process of the steel was optimized based on experiment, which is dehydrogenation annealing after forging, and then normalizing at 900°C, and tempering at 350°C. The mechanical properties of the bainitic steel is improved obviously as compared with that of commercial bainitic steel. The susceptibility of hydrogen embrittlement of the W-Al-containing steel is lower than that of commercial Mo-containing steel. The expected life time and service safety of the W-Al-containing steel crossing is higher than that of the commercial Mo-containing steel crossing.