Abstract:Bi4-xLaxTi3O12 (BLT, x=0, 0.75, 1, 2) ceramic powders were prepared with sol-gel and solid phase reaction processes, respectively. BLT powders were synthesized after decarbonization at 300 degrees C for 1h followed by calcination at 800 degrees C for 2h. The ceramics synthesized with cold isostatic pressing and sintering at 1150 degrees C exhibit a perovskite-like structure. The influence of sintering parameters and La doping content on density, microstructure and dielectric properties of the BLT were discussed. With the increase of La doping content in Bi4-xLaxTi3O12, dielectric constant increases and dielectric loss gradually decreases. The dielectric constant and dielectric loss of Bi4-xLaxTi3O12 (x=2) are 132.7 and 0.012 at 100 KHz, respectively.