Abstract:In this paper, Ti-45Al-5.5(Cr, Nb, B, Ta) alloy with sub-microstructure was prepared successfully by DMM and SPS using element powders as starting materials. XRD patterns show that the as-milled powder is mainly composed of nanometer TiAl and TiAl3 phases, and there is still Al3Ti and Ti phases to exist after DMM. The effect of sintering temperature on microstructure and properties of bulk Ti-45Al-5.5(Cr, Nb, B, Ta) alloy has been investigated. All of the samples sintered at different temperatures (900, 1000 and 1100 degrees C) exhibit high density and same phase constitution ( plenty of TiAl phase and a small quantity of Ti3Al, Ti2Al and TiB2 phases). With the sintering temperature is 900 degrees C, the sample shows good ductility, excellent yield strength and fracture strength, with the value of 5%, 1899MPa and 2229MPa, respectively. When the sintering temperature increases, the properties of the bulk Ti-45Al-5.5(Cr, Nb, B, Ta) alloy declined slightly.