Characteristics of Tungsten Inert Gas Brazing Joints of Nickel-Based Alloy and Stainless Steel

宋建岭,林三宝,杨春利,范成磊
DOI: https://doi.org/10.3321/j.issn:1004-0609.2008.05.014
2008-01-01
The Chinese Journal of Nonferrous Metals
Abstract:The tungsten inert gas(TIG) brazing of nickel-based alloy and stainless steel using CuSi3 wire was carried out.The microstructures and mechanical properties of the joint were studied using OM,SEM,EDS,instron-testing machine and hardness measurement device.The results show that the joint has dual characteristic and is divided into a welding part on the stainless steel and a brazing part on the nickel-based alloy.The stainless steel fusion zone is made of Fe-based solid solution,the interface reaction layer is made of molten unmixed zone,Ni-based fir-tree crystal microstructure and Cu-based solid solution in the intergranular.The weld is made of α-copper matrix and Fe-based solid solution in the matrix.The shear strength reaches 195 MPa and the shear fracture occurs at the interface between brazing alloy and stainless steel.The microhardness in the Ni-based fir-tree crystal,the Fe-based solid solution of the fusion zone and Cu-based solid solution of the weld near the interface reach HV433.3,HV453.4 and HV150,respectively.
What problem does this paper attempt to address?