Effect of Cooling Rate on Superfine Ti-O Inclusion Precipitation During Directional Solidification

Wang Liwei,Zheng Shaobo,Zheng Qing,Li Huigai,Zhai Qijie
DOI: https://doi.org/10.3321/j.issn:0412-1961.2007.06.008
IF: 1.797
2007-01-01
ACTA METALLURGICA SINICA
Abstract:Directional solidification method was used to simulate the precipitation of Ti-O inclusions in the sample prepared by pure Fe and Ti-Fe alloy as solute enrichment among secondary dendrites, and the effects of cooling rate on the size, number and distribution of the inclusions were investigated, furthermore the coupled model describing the relationship of microsegregation and Ti-O inclusion precipitation during solidification of liquid steel has been verified. The experimental results indicate that the inclusion size was reduced, the number increased and the distribution was more homogeneous when cooling rate was enhanced. When the cooling rates were 10, 100 and 200 K/min, the average diameters of inclusions were 1.87, 1.09 and 0.82 mu m, and the numbers were 0.31x10(4) 1.98x10(4) and 3.27x10(4) mm(-3), repectively. It has been proved that superfine inclusions can be precipitated during solidification by solute enrichment.
What problem does this paper attempt to address?