Experimental Study on the Catalytic Decomposition of Hydrogen Iodide for SI Thermochemical Cycle

Jun-hu ZHOU,Yan-wei ZHANG,Zhi-hua WANG,Wei-juan YANG,Zhi-jun ZHOU,Jian-zhong LIU,Ke-fa CEN
DOI: https://doi.org/10.3321/j.issn:1671-4431.2006.z1.023
2006-01-01
Wuhan Ligong Daxue Xuebao/Journal of Wuhan University of Technology
Abstract:Platinum was inserted into the lattice of Ce0.50Zr0.49 and Ce0.50Zn0.49 solid solution by sol-gel method to prepare 1% Pt0.01/Ce0.50Zr0.49 and Pt0.01/Ce0.50Zn0.49 catalysts. The samples were characterized by BET, XRD, SEM and experimental system of HI catalytic decomposition. The main peaks of the XRD pattern of Pt0.01/Ce0.50Zr0.49 are consistent with the characteristic peaks of cubic CeO2, which indicates the formation of CeO2-ZrO2 mixed oxides with Zr4+ replacing Ce4+ in the CeO2 lattice. The main peaks of Pt0.01/Ce0.50Zr0.49 XRD pattern are respectively consistent with the characteristic peaks of CeO2 and ZnO. The results of SEM are consistent with the results of BET and XRD. The effect of catalysts in [1] are better than our catalysts at the temperature below 450 °C. As temperature increased, Pt0.01/Ce0.50Zr0.49 and Pt0.01/Ce0.50Zn0.49 become better. HI conversions respectively achieve 32.9 % and 33.75 % at 550 °C.
What problem does this paper attempt to address?