Low Thermal Conductivity for Sr1−xLaxTiO3
G. H. Zheng,Z. X. Dai,Y. Q. Dong,F. L. Zan,D. Zou,Y. Q. Ma,G. Li
DOI: https://doi.org/10.1179/1433075x12y.0000000039
2012-01-01
Materials Research Innovations
Abstract:N type thermoelectric materials Sr1-xLaxTiO3 (x=0.02, 0.06 and 0.10) have been obtained by hydrothermal method and sintering at 900 and 1100 degrees C. The thermoelectric properties have been measured, and all of the samples in the measured temperature range have been found to be insulating. Very low thermal conductivity kappa=0.75 W m(-1) K-1 is found at 500 K for Sr0.9La0.1TiO3 after sintering at 900 degrees C. With increasing doping level x, the thermal conductivity kappa decreases. With increasing sintering temperature, the grain size of samples increases, and the thermal conductivity increases. This phenomenon is ascribed to the strong suppression of the electron and phonon conductivities due to scattering by the numerous grain boundary scattering.