Study on the protecting effect of HFC134a on AZ91D magnesium alloy in a sealed melting furnace

ShuHong Nie,Shoumei Xiong,Xiaolong Liu
2006-01-01
Abstract:The effects of holding time, temperature, furnace seal quality and stirring on the protection of AZ91D magnesium alloy were investigated in a sealed melting furnace under residual air and. N2 atmosphere containing 0.01%vol. HFC134a filled once before the experiments. The morphology, thickness, and composition of the surface film were also studied. The results showed that the highest protecting temperature was 856 C. At 760 degrees C, the effective protection time for AZ91D melt exceeded 10 hours, and the allowable pressure rising velocity in crucible exceeded 10000Pa/min. With surface stirring at a temperature lower than 800 degrees C, the new protective films were formed quickly. With the increase of the holding time and temperature, the Carbon content in surface films decreased quickly to zero, and the oxygen content increased. The morphology of all protective surface films was a compacted cellular structure with an evenly distributed thickness of about 1-2 pm, whereas that of unprotective films was wadding like structure.
What problem does this paper attempt to address?