Hot Compression Behavior of Liquidus Casting ZK60 Magnesium Alloy

HT Zhou,XQ Zeng,LF Liu,QD Wang,YP Zhu,WJ Ding
DOI: https://doi.org/10.4028/www.scientific.net/msf.488-489.563
2005-01-01
Materials Science Forum
Abstract:A ZK60 alloy made through liquidus casting is subjected to hot compression test at temperatures ranging from 513 K to 663 K and strain rates from 0.001s(-1) to I s(-1). Experimental results show that liquidus casting leads to grain refinement and granularment of alpha-Mg and promotes much more beta( Mg2Zn3) phase precipitation. During hot deformation, flow softening is found to occur and all flow stress curves exhibit a peak at temperatures and strain rates studied. The deformation activation energy of the liquidus casting ZK60 is determined to be in range of 140-198 KJ/mol. Dynamic recrystallization (DRX) occurs through which the grains are refined.