Machinable Ti3AlC2 Ceramics Produced by Spark Plasma Sintering

郭俊明,陈克新,刘光华,周和平,宁晓山
DOI: https://doi.org/10.3321/j.issn:1002-185X.2005.01.030
2005-01-01
Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Abstract:Machinable ceramics consisting of SHS Ti3AlC2 powders were first studied by Spark Plasma Sintering (SPS). Relative density of sintered Ti3AlC2 sample obtained at 1450°C and 20 MPa 5 min under vacuum is 98.4%. Sample sintered at 1500°C is full dense. The Vickers hardness of sintered Ti3AlC2 samples is enhanced with the increase of sintering temperature(1300°C-1500°C ). The SEM micrographs show that the layered grain size of sintering sample sintered by SPS increase with sintering temperature.