Machinable and mechanical properties of sintered Al 2 O 3 -Ti 3 SiC 2 composites

Yongming Luo,Shuqin Li,Wei Pan,Jian Chen,Ruigang Wang
DOI: https://doi.org/10.1023/B:JMSC.0000025843.83195.3b
IF: 4.5
2004-01-01
Journal of Materials Science
Abstract:Two-phase composites consisting of (1 − x ) Al 2 O 3 and x Ti 3 SiC 2 ( x = 0−1) were prepared by spark plasma sintering (SPS). Sintered densities larger than 98% of theoretical density were achieved when the specimens were sintered at 1300°C for 5 min (in vacuum, at pressure 30 MPa). When content of Ti 3 SiC 2 increased up to 30 wt%, composites were found to be machinable—they could be drilled easily using conventional Fe-Mo-W drills or gravers. The mechanical properties of the (1 − x ) Al 2 O 3 − x Ti 3 SiC 2 composites were evaluated. The bending strength, Vickers hardness of the specimens had the following ranges: 428 ± 10.2 ( x = 0) to 673 ± 15.4 Mpa ( x = 1) (bending strength at room temperature); 19.9 ( x = 0) to 4.0 GPa ( x = 1) (Vickers hardness).
What problem does this paper attempt to address?