Effect of La, Fe( or Co)/Ti on Aging Characteristic of Copper Alloys

FX Huang,JS Ma,ZT Geng,HL Ning,HG Suzuki,SM Guo,XT Yu,T Wang,H Li,XC Li
DOI: https://doi.org/10.3321/j.issn:1002-185x.2004.03.011
2004-01-01
Rare Metal Materials and Engineering
Abstract:The effect of La, Fe(or Co)/Ti on the aging characteristics of Cu-Cr-Zr-Zn alloys were investigated. The results showed that the peak hardness and strength of Cu-Cr-Zr-Zn alloy and Cu-Cr-Zr-Zn-La alloy occurs at about 450degreesC for 2h after solution treated and followed by 70% reduction which is HV 1 770 MPa, 525 MPa and HV 1 840 MPa, 554 MPa, respectively. The peak hardness and strength of Cu-Cr-Zr-Fe-Ti-Zn-La alloy and Cu-Cr-Zr-Co-Ti-Zn-La alloy occurs at about 450degreesC for 2h after solution treated and followed by 70% reduction and aged at 500degreesC for 2 h and cold worked by, which is HV 2 120 MPa, 683 MPa, and HV 2 040 MPa, 651 MPa, respectively.