Microstructure of Sm 2 Co 17 Magnets and Its Influence on Coercivity

LY Li,JH Yi,BY Huang,YD Peng,J Du
2004-01-01
Abstract:Sm(Coba1 Fe0.197Cu0.049Zr0.026)7.5 magnet with Hci of 2105 kA/m andβ18-200℃ of - 0.17%/℃ was made by sintering processing. The magnet has uniform celluler structure. The cell interior is a rhombohedarl 2:17phase,and the boundary is a hexagonal 1:5 phase. The average cell size is 93 nm and the cell boundary thickness is 20 nm.The cells are enriched in Fe,and the cell boundaries are enriched in Cu. More Cu-riched 1:5 cell boundary phase would be helpful to obtain a higher coercivity and lower temperature coefficient. White secondary phase mainly consisting of Sm can decrease the coercivity of the magnets, but the closely paralleled grooves can increase coercivity.