CORROSION OF SUPERALLOY GH132 TUBE IN THE ENVIRONMENT OF DISPOSING PROPELLANT WASTEWATER BY SUPERCRITICAL WATER OXIDATION

张丽,韩恩厚,柯伟
DOI: https://doi.org/10.3969/j.issn.1005-4537.2004.02.014
2004-01-01
Abstract:Corrosion behavior of a candidate connecting tube,a GH132 tube,for supercritical water oxidation(SCWO)system in the environment of disposing the propellant wastewater by SCWO method with the range of temperatures from room temperature to 520℃ and the pressure of 27.2 MPa was studied.The morphology of corrosion surface was analyzed using SEM.Intergranular corrosion (IGC) and shallow pitting occurred respectively when the temperature was above 180℃ and 260℃.Severe stress corrosion cracking was found at 280℃ which led to leak of the tube after 151 h of testing.The maximum decrease in wall thickness of the tube was measured between 340℃ and 370℃,which amounted to 100μm.Within the supercritical temperature range,corrosion of the tube was obviously mitigated and only very shallow pits could be found.Corrosion products were analyzed using EDX and Fourier transfer infrared spectrometry (FTIR).The selective dissolution of elements such as Fe,Cr and Ni and the formation of corresponding oxides and hydroxides accelerated general corrosion within the subcritical temperature range,while,in the supercritical temperature range,corrosion products was protective due to their very low solubilities.Results showed that GH132 tubes could not be used as connecting tubes at subcritical temperatures.
What problem does this paper attempt to address?