Low-Friction MoS x Coatings Resistant to Wear in Ambient Air of Low and High Relative Humidity

Xiaoling Zhang,B. Prakash,W. Lauwerens,Xiaodong Zhu,Jiawen He,J.-P. Celis
DOI: https://doi.org/10.1023/A:1021760405423
2003-01-01
Tribology Letters
Abstract:The investigation of the tribological performance of MoS 2 -based coatings in air of high humidity is critical for the future use of such low-friction and high-wear-resistant coatings in ambient air. Sulfur-deficient MoS x coatings with a basal plane ( x = 1.3) and a random ( x = 1.8) crystallographic orientation were produced by planar magnetron sputtering. The coefficient of friction and the wear loss of MoS x coatings in comparison with TiN and amorphous TiB 2 coatings were investigated in bi-directional sliding fretting tests performed in ambient air of different relative humidity. The wear rate expressed as a volumetric loss per unit of dissipated energy was determined. From these results, the best friction and wear performance was achieved with basal-plane-oriented MoS x coatings tested at a relative humidity in the range of 10-50%. A coefficent of friction of 0.06-0.08 and a wear rate of 4 × 10 3 μ m 3 J -1 , at a normal load of 1 N and a fretting frequency of 10 Hz, were recorded for that type of MoS x coatings.
What problem does this paper attempt to address?