Mn-SR As an Ozone Catalyst for Coal to Ethylene Glycol Organic Wastewater Treatment: Activity Evaluation and Reaction Mechanism
Nan Zhang,Yingying Dong,Ye Yang,Zhiwen Chen,Kanfolo Franck Herve Yeo,Wei Tian,Liu Han,Wendong Wang
DOI: https://doi.org/10.1016/j.jece.2023.110701
IF: 7.7
2023-01-01
Journal of Environmental Chemical Engineering
Abstract:Large amounts of soda residue waste from the production of sodium carbonate industries cause serious pollution to environment. In this study, a novel Mn-SR non-homogeneous ozone catalyst was prepared by mixed calcination method using soda residue as the main component for organics degradation of coal to ethylene glycol wastewater. Firstly, under the optimal Mn-SR preparation process (95% n-SR (m(soda residue): m(kaolin) = 8:1), 5% MnO2, calcination temperature: 500 degrees C, calcination time: 4 h) and the optimal operating conditions (pH: 8, water temperature: 40 degrees C, catalyst dosage: 320 g/L, O-3 dosage: 20 g/L) for the reaction of 60 min, the COD removal rate reaches to 77.1%, which is 63.9% higher than only ozonation COD removal efficiency under the same conditions. Kinetic study shows that water temperature is the most important factor affecting COD degradation rate in the reaction system. Through the adsorption performance, ozone utilization, free radical quenching experiments and three-dimensional fluorescence tests, the catalytic performance of Mn-SR catalysts for ozonation was investigated. The results showed that Ca and Mg in Mn-SR play a major role in organics degradation, while MnO2 plays a complementary role in the degradation of high COD concentrations. It was confirmed that hydroxyl radicals (center dot OH) are the main reactive radicals in the Mn-SR catalytic ozonation system, which plays an important role in the degradation of organics in wastewater. Meanwhile, after Mn-SR was reused and regenerated for five times, the COD removal rates was still higher than 67.0%, and Mn-SR recovery rates were more than 94.7%, which showed a good stability.