Effect of temperature on the friction and wear properties of a crosslinked and a linear polyimide

Peihong Cong,Tongsheng Li,Xujun Liu,Xushou Zhang,QunJi Xue,Jiaze Li
DOI: https://doi.org/10.3321/j.issn:1000-3304.1998.05.008
1998-01-01
Acta Polymerica Sinica
Abstract:The effect of temperature on the friction-wear properties of a kind of liner Polyimide (YS-20) and a kind of crosslinked Polyimide (KH-304) was studied using a pinon-disc wear tester. The test results showed that with sliding time increasing, friction coefficient of YS-20 increased to a maximum then decreased to steady value, but that of KH-304 decreased directly to steady value. For a steady value of friction coefficient, with temperature increasing, the friction coefficient of YS-20 increased to a maximum value then decreased, but that of KH-304 decreased directly to steady value. Wear rate of the both Polyimides (Pis) increased with temperature increasing. The wear rate of KH-304 was higher than that of YS-20 under the same temperature. Scanning Electron Micrograph (SEM) analysis indicated that with temperature elevating, debris of YS-20 appearances changed obviously, but that of KH-304 varied little. Fourier Transform infrared Spectrometer (FTIR) indicated that the tribochemical reaction of KH-304 occurred more obviously than that of YS-20. The analysis above suggest that the surface layer of the linear PI changed from glassy body, to elastomer and then to melting body. Tribochemical reaction occurred at the surface of the crosslinked PI, which effect the friction-wear properties of the linear PI and crosslinked PI respectively.
What problem does this paper attempt to address?