Effects of thermal treatment on the mechanical properties of poly(p-phenylene benzobisoxazole) fiber reinforced phenolic resin composite materials

Liping Bian,Jiayu Xiao,Jingcheng Zeng,Suli Xing,Changping Yin,Aiqing Jia
DOI: https://doi.org/10.1016/j.matdes.2013.08.058
2014-01-01
Materials & Design (1980-2015)
Abstract:•The PBO fiber reinforced composites were heated at high temperature.•After heating at 300°C, the composites had irreversible damage due to the resin.•Above 550°C, PBO fiber pyrolyzed and affected the composite much.•After heating at 550°C, the resin matrix pyrolyzed mostly and broke the interface.•After heating at 700°C, mechanical properties of the composites decreased much.