Performance of Al–0.5 Mg–0.02 Ga–0.1 Sn–0.5 Mn As Anode for Al–air Battery in NaCl Solutions

Jingling Ma,Jiuba Wen,Junwei Gao,Quanan Li
DOI: https://doi.org/10.1016/j.jpowsour.2013.12.053
IF: 3.9
2014-01-01
Journal of The Electrochemical Society
Abstract:In this research, Al-air battery based on Al-0.5 Mg-0.02 Ga-0.1 Sn-0.5 Mn anode with industrial 2N8 aluminum was prepared, the corrosion behavior and the battery performance were investigated in 2 molL(-1) NaCl, 4 molL(-1) NaOH, 4 molL(-1) NaOH + 0.2 molL(-1) ZnO, 7 molL(-1) KOH and 7 molL(-1) KOH + 0.2 molL(-1) ZnO solutions. The results show that compared with in alkaline solutions, the alloy has higher electrochemical performance and lower self-corrosion rate in 2 molL(-1) NaCl, the corrosion potential and the self-corrosion rate of the alloy in 2 molL(-1) NaCl are -1.401 V (vs Hg/HgO) and 0.0008 cm year(-1), respectively. At a current density of 20 mAcm(-2), the operate voltage of Al-air battery is 1.116 V, and the anodic utilization rate is 83.7% in 2 molL(-1) NaCl. The morphology after discharge is passivity attributed to the surface hydroxide layer on the alloy in 2 molL(-1) NaCl. The high anodic utilization during discharge in 2 molL(-1) NaCl is partially responsible for the higher Rt, which is well validated by EIS measurement. (C) 2014 The Electrochemical Society. All rights reserved.
What problem does this paper attempt to address?