Effect of Ce on microstructure and deformation performance of ZK20 alloy

Quan Li,Jian Peng,Renju Cheng,Wenjun Liu,Bin Zeng,Xianquan Jiang,Fusheng Pan
2013-01-01
Abstract:The effects of different Ce contents on the microstructure, mechanical properties and performance of hot deformation were investigated. By methods of OM, X-ray, SEM, XRD, tensile test at room temperature and hot compression test on Gleeble 1500D thermal-mechanical simulator, the mechanism properties of Ce element in ZK20 and its effect on microstructure were analyzed. The results showed that within the experimental range (0 to 0.68% Ce (mass fraction, the same below)), the phase τ were increased with the addition of Ce, the form were changed to the discontinuity mesh and mesh in the alloy by hot extrusion. Ce element could improve the recrystallization of the alloy. The grain size continuously decreased with increasing Ce. The extruded alloy exhibted best mechanical properties with the 0.7% addition of Ce. Its room temperature tensile strength was 261 MPa, yield strength was 198 MPa, elongation was 24.6%. Annealing process in condition of 280°C and 4 h could contribute to the strength and ductility of the alloy. Its tensile strength was improved to 272 MPa, yield strength was improved to 209 MPa, and elongation was 26%. The addition of Ce into ZK20 alloy could cause the transition of brittle fracture to brittle and dimple mixed fracture.
What problem does this paper attempt to address?