Abstract:The treatment of reductive laterite by corrosion process was studied using the laterite processed by chloridizing segregation process as starting materials. The effects of mass ratio of acid to ore, air flux, leaching temperature, leaching time, stirring speed, and solid-to-liquid ratio (ratio of solid mass to liguid volume, g/mL) on the leaching rates of Fe, Ni and Co were systematically investigated. The results show that under the optimum conditions of mass ratio of acid to ore 0.1:1, air flux 1 L/min, leaching temperature 80 ℃ and time 8 h, stirring speed 300 r/min, solid-to-liquid ratio 1:10, the leaching rates of Ni and Co are respectively 90.9% and 80.2%, and the leaching rate of Fe is only 9.9%. Consequently, Ni and Co can be effectively separated from Fe.