Microstructure Evolution of Sub-Critical Annealed Laser Deposited Ti–6Al–4V Alloy

Y. Lu,H. B. Tang,Y. L. Fang,D. Liu,H. M. Wang
DOI: https://doi.org/10.1016/j.matdes.2011.12.016
IF: 9.417
2012-01-01
Materials & Design
Abstract:Laser deposited titanium alloy Ti-6Al-4V was sub-critically annealed in the alpha + beta phase region and the microstructure evolution process and microstructure characteristics were systematically investigated as functions of annealing temperature and time during the sub-critical annealing process. A unique bimodal microstructure consisting of coarse crab-like primary alpha and fine lamellar transformed beta is obtained by sub-critical annealing in the upper part of alpha + beta phase region. The crab-like morphology of the primary alpha becomes more manifest with the increasing anneal temperature up to its beta-transus temperature. The annealing treatment has significant effect on the volume fraction, size and aspect ratio of primary alpha, while the aging treatment mainly affects the volume fraction and aspect ratio of primary alpha and the width and volume fraction of secondary alpha. Formation of the crab-like primary alpha is due to the preferential epitaxial growth of secondary alpha on the edge of primary alpha along with the < 1210 > preferred crystallographic direction during the diffusive beta-decomposition process. The sub-critically annealed alloy exhibited the maximum microhardness by further aging at approximately 600 degrees C, which is 9% higher than that of the as-annealed one and 4% higher than the as-deposited one. (C) 2011 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?