Effects of Zr Addition on As Cast Microstructure, Tensile and Creep Properties of Mg–3·8Zn–2·2Ca Magnesium Alloy

J. M. Peng,M. B. Yang,Y. Zhu,F. S. Pan
DOI: https://doi.org/10.1179/1743133612y.0000000003
2012-01-01
International Journal of Cast Metals Research
Abstract:The effects of Zr addition on the as cast microstructure, tensile and creep properties of Mg-3.8Zn-2.2Ca (wt-%) magnesium alloy were investigated. The results indicate that adding 0.19-0.81 wt-% Zr to the Mg-3.8Zn-2.2Ca does not cause the formation of any new phases but causes the morphology of the Ca2Mg6Zn3 phase to change from the initial continuous and/or quasi-continuous net to the quasi-continuous and/or disconnected shapes. Furthermore, adding 0.19-0.81 wt-% Zr can effectively refine the grains of the Mg-3.8Zn-2.2Ca alloy, and an increase in Zr amount from 0.19 to 0.81 wt-% causes the grain size to gradually decrease. In addition, adding 0.19-0.81 wt-% Zr to the Mg-3.8Zn-2.2Ca alloy can improve the tensile properties but decreases the creep properties. Among these Mg-3.8Zn-2.2Ca alloys with the additions of 0.19, 0.52 and 0.81 wt-% Zr, the alloy with the addition of 0.81 wt-% Zr exhibits the relatively optimal tensile and creep properties.
What problem does this paper attempt to address?