Abstract:Dense MgB2 wires were successfully fabricated through the in-situ powder-in-tube (PIT) method by using steel sheath with low carbon content. Short samples of MgB2/Fe wires were sintered at 650-850 degrees C for 2-5 hours in argon. Critical current density(J(c)) of the wires was measured at 4.2K in the magnetic field up to 8 T by standard four probe method. High J(c) values of 2.1x10(5)A/cm(2) in 3T at 4.2K were obtained for MgB2/Fe wires. The microstructure observation for MgB2 wires showed that no reaction between Fe and MgB2 was found and MgB2/Fe wires had better grain connectivity. The results indicated that the J(c) can be further improved to meet the requirement for applications by optimizing the process conditions.
What problem does this paper attempt to address?