Influence of Nitrogen on the Catalytic Behaviour of Pt/γ-Al2O3 Catalyst in Glycerol Reforming Process

Nian-Jun Luo,Jin-An Wang,Tian-Cun Xiao,Fa-Hai Cao,Ding-Ye Fang
DOI: https://doi.org/10.1016/j.cattod.2010.04.013
IF: 5.3
2011-01-01
Catalysis Today
Abstract:In the present work, deactivation behaviour of a Pt/γ-Al2O3 catalyst used for converting glycerin/water mixture into hydrogen was investigated. It was shown that main reason for the catalyst activity drop is due to the carbon deposition over the catalyst surface. Interestingly, the catalyst suffered from faster deactivation in the case of nitrogen presence in the inlet stream. However, the catalytic stability of the catalyst could be greatly enhanced when nitrogen was phase out from the reaction atmosphere. In the reaction mixture containing 10wt% glycerol, the deactivation constant of the catalyst decreased from dA=−0.0516mL/(mingcat.h) under a condition with nitrogen to dB=−0.0051mL/(mingcat.h) without nitrogen in the reaction bed. Catalytic evaluation and thermogravimetric analysis revealed that nitrogen was not only an inert carrier gas served as but also an accelerator for coking. A speculation model was proposed for explanation of the coking process over the catalyst with the nitrogen effect.
What problem does this paper attempt to address?