Isothermal Compression of the Alloys of Iron Up to 300 Kilobars at Room Temperature: Iron-nickel Alloys

T TAKAHASHI,WA BASSETT,HK MAO
DOI: https://doi.org/10.1029/jb073i014p04717
1968-01-01
Journal of Geophysical Research
Abstract:Journal of Geophysical Research (1896-1977)Volume 73, Issue 14 p. 4717-4725 Isothermal compression of the alloys of iron up to 300 kilobars at room temperature: Iron-nickel alloys Taro Takahashi, Taro TakahashiSearch for more papers by this authorWilliam A. Bassett, William A. BassettSearch for more papers by this authorHo-Kwang Mao, Ho-Kwang MaoSearch for more papers by this author Taro Takahashi, Taro TakahashiSearch for more papers by this authorWilliam A. Bassett, William A. BassettSearch for more papers by this authorHo-Kwang Mao, Ho-Kwang MaoSearch for more papers by this author First published: 15 July 1968 https://doi.org/10.1029/JB073i014p04717Citations: 110AboutPDF ToolsRequest permissionExport citationAdd to favoritesTrack citation ShareShare Give accessShare full text accessShare full-text accessPlease review our Terms and Conditions of Use and check box below to share full-text version of article.I have read and accept the Wiley Online Library Terms and Conditions of UseShareable LinkUse the link below to share a full-text version of this article with your friends and colleagues. Learn more.Copy URL Share a linkShare onFacebookTwitterLinkedInRedditWechat Abstract The effect of pressure on the crystal structure and the molar volume of iron alloyed with 5 and 10% nickel was determined up to 300 kb at room temperature by means of X-ray diffraction techniques employing a diamond-anvil high-pressure cell. The alloys undergo a reversible bcc-hcp phase transformation, which is accompanied by a volume change of −0.36 ± 0.02 cm3/mole. The crystallographic axis ratio, c/a, of the hcp phase appears to increase with nickel content, whereas it appears to be unaffected by pressure. The bulk moduli calculated from the volume data for the bcc and hcp phases of the alloys do not differ significantly from those for the respective phases of iron. The bulk modulus value for the hcp phase evaluated at zero pressure has been calculated to be 2.06 ± 0.15 Mb and is about 20% greater than that for the bcc phase. The volume of the hcp phase at zero pressure has been calculated from the pressure-volume data by extrapolation. A value of 6.67 ± 0.02 cm3/mole has been obtained for iron and the alloys. The pressure-volume relationship obtained by this work is consistent with the results obtained by R. G. McQueen and S. P. Marsh (1960, 1966) using shock compression techniques. Citing Literature Volume73, Issue1415 July 1968Pages 4717-4725 RelatedInformation
What problem does this paper attempt to address?