Abstract:In situ consolidation colloidal-forming processes, such as gelcasting, are promising techniques for complex shaping of materials with high density, high uniformity and, thus, high reliability of performance. Non-oxide powders, e.g. Si, SiC and Si3N4, are suitable for being well dispersed in alkaline solutions. However, silicon powder and free silicon contained in silicon carbide and silicon nitride powders have a tendency to hydrolize, especially in a basic aqueous solution for gelcasting, causing a large amount of macropores in green bodies as a consequence of hydrogen gas evolution. Moreover, silicon nitride itself is chemically unstable in aqueous solutions and reacts with other reagents when processed by aqueous gelcasting, which also affects the microstructure of green bodies. After identifying the causes of macropore formation in the gelcast green bodies, some solutions are proposed to overcome these problems.