EFFECT OF WATER ON DIELECTRIC PERFORMANCES OF ALKALI ACTIVE SLAG CEMENT MATERIALS(Ⅰ)

CUI Xuemin,QIU Shuheng,CAO Deguang,ZHOU Ji
DOI: https://doi.org/10.3321/j.issn:0454-5648.2007.06.026
2007-01-01
Abstract:Dielectric performances of hardening alkali active slag cement(AASC)paste were studied.The experimental results show the drying method(100℃for 4 h)that could depress the effect of free-water on the dielectric performances of the AASC.The dielec-tric frequency also shows the dielectric constant(εr)is 6—8 and the dielectric loss(tanδ)is 0.02—0.04 at high frequency.With the increase of deposition time in air with a relative humidity of about 40%,the AASC would absorb the water vapor in the air.The satu-rated absorption is about 1.2%in mass(the same below),so theεr and tanδincreased rapidly.Therefore,the low temperature drying method could not completely eliminate the absorption of the AASC paste.In addition,the dried AASC paste still contained about 2% hydrate water of hydration that was proved by the differential thermal analysis and thermogravimetry analysis,so,the tanδof the AASC paste was higher than ceramic material.
What problem does this paper attempt to address?