INFLUENCE OF ACTIVATION TEMPERATURE ON METAL-SUPPORT INTERACTION IN NiW/Al2O3 CATALYST

Hong Nie,Xiangyun Long,Qinghe Liu,Dadong Li
DOI: https://doi.org/10.3969/j.issn.1005-2399.2010.07.001
2010-01-01
Abstract:The influence of activation temperature during the preparation of NiW/Al_2O_3 catalysts on the metal-support interaction was studied.Test results show that the activation temperature has significant effect on the hydrodesulfurization(HDS)activity of the catalyst when using 4,6-dimethyldibenzothiophene as model compound;the optimum activation temperature is in the range of 350℃ to 400℃,catalysts activated in this temperature range exhibited high HDS activity due to the moderate metal-support interaction and a promotion to the sulfidation of W species,which are well supported by the results of UV-Vis,H_2-TPR and XPS characterization. High temperature(>450℃)activation may cause a strong metal-support interaction,which leads to the formation of Ni-Al spinel and the decomposition of Ni-W-O mixture,and that might further suppress the sulfidation of W species,as a result,the catalyst activity is reduced.
What problem does this paper attempt to address?