Preparation and Oxygen Release Properties of Calcium Peroxide-based Oxygen Slow-release Composite

Yan-bo ZHOU,Ying-xiu WANG,Zhen-hua ZHOU,Yang LI,Jun LU
DOI: https://doi.org/10.3969/j.issn.1000-4602.2012.07.015
2012-01-01
Abstract:Stearic acid was used to embed calcium peroxide under anhydrous conditions in order to prepare an oxygen slow-release composite that supplies oxygen for water environment remediation.The infrared spectroscopy and scanning electron microscopy confirmed that stearic acid could effectively embed calcium peroxide,and the surface of oxygen slow-release composite was more closely and flat than before.Based on the tests in aseptic and oxygen-free water,it was found that the oxygen release rate decreased with the stearic acid concentration increase,and the pH value also leveled off.The results from the simulation sediment showed that with calcium peroxide dosage of 720 g/m2,the oxygen slow-release composite(stearic acid content of 1.2%) maintained the dissolved oxygen concentration around 5.0 mg/L within 42 d at 25 ℃,and pH value gradually reduced from 8.7 to 7.7 relying on sediment self-buffering,which was conducive to microbial growth and inhibition of endogenous pollutants release.
What problem does this paper attempt to address?