Abstract:Objective:To determine the ultimate tensile strength(UTS) of molar coronal dentin and the dentin-enamel junction(DEJ) area,and analyze its fracture surface.Methods: A resin composite block was built up on the human third molar occlusal surface.Slice the teeth buccolingually to obtain slices about 1mm thick.Each slice was then trimmed to a dumbbell-shaped specimen with a fine diamond bur,and to reduce a cross sectional area of about 1mm×1mm.DEJ,superficial dentin,middle dentin and deep dentin specimens were obtained from the midcoronal for tensile testing vertically and horizontally.The fracture surfaces were observed by scanning electron microscope.Results:The UTS of dentin at different levels was anisotropic and decrease from superficial dentin to deep dentin(P0.05).The UTS of DEJ and middle dentin showed no significant difference(P0.05).SEM micrographs:Fractures did not occur in one single plane along the peritubular dentin and intertubular dentin.The direction of fracture crack was changed in the dentin and enamel.Most DEJ specimens fractured in the nearby enamel.Conclusions:The dentin of molar crown showed higher ability to resistant fracture in the horizontal direction.The dentin-enamel junction provided a crack-arrest barrier for flaws formed in the brittle enamel.
What problem does this paper attempt to address?