PREPARATION AND PROPERTIES OF HIGH TEMPERATURE SELF LUBRICATING COATINGS BY INDUCTION SINTERING

Xiao Ling,Ding Chunhua,Sun Yanhua,Yu Lie
DOI: https://doi.org/10.3724/sp.j.1037.2010.00585
IF: 1.797
2011-01-01
ACTA METALLURGICA SINICA
Abstract:NiCr-based self-lubricating PM304 coatings have been used successfully in many high-temperature, high-speed applications such as air cycle machines, bleed air turbo compressors and turbo expanders. However, coarse PM304 coatings are not fully dense, containing a few percentages of pores and cracks which are harmful not only to the coating's tribological properties but also to the coating's overall mechanical strength. Furthermore, fine IS304 was prepared by the methods of high energy ball milling and induction sintering. The size of self-lubricating phase was refined, with Ag particles of about 5 mu m and BaF2/CaF2 of about 1 mu M. The results show that temperature and microstructure have a great effect on wear properties of IS304 and PM304 coatings. At the temperature of 20-340 degrees C, the friction coefficients of two types of coatings (IS304 and PM304) are higher, and the microscopic brittle fracture is the dominant wear mechanism. With the increase of the temperature, the coefficient of the coatings decreases rapidly due to the formation of self-lubricating film on the worn surfaces which consist of Ag and fluoride. At the temperature of 340-700 degrees C, since the self lubricating phase is fine and uniformly distributed in the IS304 coatings, it makes the formation of an intact lubricating film as well as Ag film fine and well distributed. Thus, the friction coefficient of IS304 is lower than that of PM304. With a further increase at the temperature of 700-800 degrees C, there is the plastic flow on the surfaces of the softened self-lubricating film under the influence of the friction force. Consequently, the friction coefficients of the coatings increase obviously. Comparing the PM304 with IS304 coatings, as the size of Ag film is large and the plastic flow of Ag film is much more severe than that of fluoride film, the friction coefficient of PM304 is higher than that of IS304.
What problem does this paper attempt to address?