The Microstructure Parameters and Microhardness of Directionally Solidified Ti–43Al–3Si Alloy

Jianglei Fan,Xinzhong Li,Yanqing Su,Jingjie Guo,Hengzhi Fu
DOI: https://doi.org/10.1016/j.jallcom.2010.07.122
IF: 6.2
2010-01-01
Journal of Alloys and Compounds
Abstract:TiAl-based alloy (Ti–43Al–3Si at.%) was directionally solidified at a constant temperature gradient (G=20K/mm) in a wide range of growth rates (5–60μm/s) by using a Bridgman type directional solidification furnace. The cellular spacing (λ), lamellar spacing (λL), volume fraction of Ti5Si3 phases (fV) and microhardness (HV) were measured. The values of λ, λL and fV decrease with increasing growth rate (V). The value of HV increases with the increasing values of V and λL−0.5, and decreases with the increasing values of λ, and fV. The dependence of HV on V, λ, λL−0.5 and fV was determined by linear regression analysis. The fitted exponent values obtained in this work were compared with the previous experimental results for similar alloy systems.
What problem does this paper attempt to address?