Experimental research on strength of synthetic fiber reinforced concrete after high temperatures

Wang Yuehua,Ding Yining
2008-01-01
Abstract:The compressive strength and the flexural strength of Normal Concrete(NC),Polypropylene Fiber Reinforced Concrete(PPFRC) and Polyacrylonitrile Fiber Reinforced Concrete(PANFRC) under normal temperature and after different high temperatures of 300℃,600℃,(1 000)℃ are investigated,and the influences of different high-temperature heating methods and loading conditions are analyzed. The results show that,the deterioration of concrete under high temperature of 300℃ is mainly influenced by heating rate,while the deterioration of concrete under high temperature upwards of 600℃ is mainly influenced by temperature.Mixing PP fiber or PAN fiber with low content can mitigate the high-temperature deterioration of concrete,with the result of improving the compressive strength of concrete after high temperature and also improving the flexural strength of concrete when loading on the unexposed surface after fire.
What problem does this paper attempt to address?