Preparation and Particle Sizes Controlling of Cuprous Oxide Microcrystals by Homogeneous Reduction

ZHAI Jiwei,GAO Rongjie,JIANG Kuiguang,SUN Mingzhi
DOI: https://doi.org/10.3321/j.issn:1005-023X.2009.18.031
2009-01-01
Abstract:Cuprous oxide microcrystals are prepared by homogeneous reduction using CuSO4·5H2O and Na2SO3.All the powders are characterized by X-rays diffraction(XRD),scanning electron microscopy(SEM) and Malvern Zetasizer Nano ZS laser particle size analyzer.The results show that all the microcrystals have even grain size and good dispersibility.The results of the orthogonal test show that there are three influencing factors on the granularity of Cu2O:reagent concentration,reaction time and temperature.The optimum conditions are 0.05mol/L(CuSO4·5H2O and Na2SO3),358K and 2h,the granularity of the powders obtained is 300nm,granularity distributing is 60nm.Diffusion and aggregation mechanisms are used to explain the formation of different granularity of cuprous oxi-de.0.3~3.0μm global cubic Cu2O is obtained through controlling the conditions.
What problem does this paper attempt to address?