Effect of Technological Conditions on Preparation of Co3O4 Powders by Solution Spray-Oxidation

郭学益,冯庆明,郭秋松,田庆华
DOI: https://doi.org/10.3969/j.issn.1673-0224.2009.05.009
2009-01-01
Abstract:High quality Co3O4 powder was prepared from CoCl2·6H2O solution by spray-oxidation method. The effects of reaction temperature, concentration of aqueous CoCl2·6H2O solution as well as atomizing air pressure on the morphology and particle size distribution of Co3O4 particles were investigated systematically. The results show that the reaction temperature has effect on both the morphology and particle size distribution of Co3O4 particles. The powder with better spherical morphology and smaller particle size can be obtained at higher reaction temperature. The concentration of aqueous CoCl2·6H2O also has effect on the particle size. The higher the concentration of aqueous CoCl2·6H2O is, the bigger the particle size is. Increasing the atomizing air pressure is beneficial for obtaining good powder size distribution and dispersity. The optimum conditions were determined: the temperature is 850 ℃; the concentration is 1.5 mol/L; the air pressure is 1.5×105 Pa. In this condition, the pure and spherical Co3O4 powder with narrow particle size distribution can be obtained.
What problem does this paper attempt to address?