Study on the Kinetics of Extracting Chrysotile with Ammonium Chloride

GAO Xiong,MENG Ye,ZHU Chen,ZHAO Liang
DOI: https://doi.org/10.3969/j.issn.1001-4810.2011.04.020
2011-01-01
Abstract:Low mineral dissolution rate and the unrecyclable use of additives are two puzzles development of CO2 sequestration by mineral carbonation.This paper presents a new process of CO2 sequestration by mineral carbonation,which adopts NH4Cl solution as leaching agent,and study the reaction kinetics of chrysotile in NH4Cl solution in a systematic way.The results show that dissolution process is in conformity with the Elovich model and leaching process is usually finished in 1 hour.The leaching rate of magnesium can reach 12.67 % when the concentration of NH4Cl is 5 mol/L and the reacting temperature is 100 ℃.And the leaching rate rise with temperature,meanwhile,neither does the ammonium chloride concentration nor the solid/liquid ratio have much influence on it.The activation energy of dissolution process is determined to be 129.56 kJ/mol in the test.
What problem does this paper attempt to address?